Customization: | Available |
---|---|
Length: | 1800mm-2700mm |
Density: | 1.58-1.66 g/cm3 |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Category | No. | Specifications | |
Diameter (mm) | Length (mm) | ||
Regular Power Graphite Electrodes | 1 | 100 | 1800 |
2 | 200 | 1800 | |
3 | 250 | 1800 | |
4 | 300 | 1800 | |
5 | 350 | 1800 | |
6 | 400 | 2000 | |
7 | 500 | 2200 | |
8 | 600 | 2200 |
Category | No. | Specifications | |
Diameter (mm) | Length (mm) | ||
High power graphite electrode | 1 | 250 | 1800 |
2 | 300 | 1800 | |
3 | 400 | 1800 | |
4 | 500 | 2200 | |
5 | 600 | 2400 | |
6 | 700 | 2700 |
Category | No. | Specifications | |
Diameter (mm) | Length (mm) | ||
Ultra high power graphite electrode | 1 | 300 | 1800 |
2 | 350 | 1800 | |
3 | 400 | 2200 | |
4 | 450 | 1800 | |
5 | 500 | 2200 | |
6 | 550 | 2300 | |
7 | 600 | 2400 | |
8 | 700 | 2700 |
Technical Properties of RegularPower Graphite Electrodes and nipple | ||||||||
Item | Classification | Unit | NominalDiameter (mm) | |||||
75-200 | 250-300 | 400-500 | ||||||
Gifted class | First level | Gifted class | First level | Gifted class | First level | |||
A | B | A | B | A | B | |||
Electric Resistivuty(<=) | Elatrode | μΩ.m | 8.0 | 9.0 | 9.0 | 9.0 | 8.0 | 9.0 |
Nipple | 7.5 | 7.5 | 7.5 | |||||
Bending strength(>=) | Elatrode | Mpa | 10.0 | 10.0 | 8.0 | |||
Nipple | 15.0 | 15.0 | 15.0 | |||||
Elastic moduluc(<=) | Elatrode | Gpa | 12.0 | 12.0 | 12.0 | |||
Nipple | 14.0 | 14.0 | 14.0 | |||||
Bulk density(>=) | Elatrode | g/cm3 | 1.58 | 1.58 | 1.58 | |||
Nipple | 1.68 | 1.68 | 1.68 | |||||
CTE(<=) | Elatrode | X10-6/ºC | 2.7 | 2.7 | 2.7 | |||
Nipple | 2.5 | 2.5 | 2.5 | |||||
Ash(<=) | % | 0.3 | 0.3 | 0.3 | ||||
Note: Ash content and thermal expansion coefficient are parameter indicators |
Technical Properties of High Power Graphite Electrodes and nipple | ||||||||
Item | Classification | Unit | NominalDiameter (mm) | |||||
300-400 | 450-500 | 550-600 | ||||||
Electric Resistivuty(<=) | Elatrode | μΩ.m | 7.0 | 7.0 | 7.0 | |||
Nipple | 6.0 | 6.0 | 5.8 | |||||
Bending strength(>=) | Elatrode | Mpa | 10.5 | 10.0 | 10.0 | |||
Nipple | 14.0 | 14.0 | 16.0 | |||||
Elastic moduluc(<=) | Elatrode | Gpa | 12.0 | 12.0 | 12.0 | |||
Nipple | 16.0 | 16.0 | 16.0 | |||||
Bulk density(>=) | Elatrode | g/cm3 | 1.62 | 1.62 | 1.62 | |||
Nipple | 1.72 | 1.72 | 1.72 | |||||
CTE(<=) | Elatrode | X10-6/ºC | 2.4 | 2.4 | 2.4 | |||
Nipple | 2.2 | 2.2 | 2.2 | |||||
Ash(<=) | % | 0.3 | 0.3 | 0.3 | ||||
Note: Ash content and thermal expansion coefficient are parameter indicators |
Technical Properties of Ultra High Power Graphite Electrodes and nipple | ||||||||
Item | Classification | Unit | NominalDiameter (mm) | |||||
300-400 | 450-500 | 550-700 | ||||||
Electric Resistivuty(<=) | Elatrode | μΩ.m | 6.2 | 6.2 | 6.3 | |||
Nipple | 5.0 | 5.0 | 4.5 | |||||
Bending strength(>=) | Elatrode | Mpa | 10.5 | 10.5 | 11.0 | |||
Nipple | 18.0 | 18.0 | 20.0 | |||||
Elastic moduluc(<=) | Elatrode | Gpa | 14.0 | 14.0 | 14.0 | |||
Nipple | 18.0 | 18.0 | 22.0 | |||||
Bulk density(>=) | Elatrode | g/cm3 | 1.66 | 1.66 | 1.66 | |||
Nipple | 1.75 | 1.75 | 1.75 | |||||
CTE(<=) | Elatrode | X10-6/ºC | 1.5 | 1.5 | 1.4 | |||
Nipple | 1.4 | 1.4 | 1.2 | |||||
Ash(<=) | % | 0.3 | 0.3 | 0.5 | ||||
Note: Ash content and thermal expansion coefficient are parameter indicators |